Dr.Vakuum
Все применения

Vacuum heat treatment and brazing furnaces: the pump set behind a bright finish

7 мин чтения

A steel part heated to 1,000 °C in air is covered in scale and has lost carbon from its surface. The same part heated in a vacuum furnace comes out bright, with its chemistry intact and its dimensions unchanged — which is why Thailand's tool-and-die shops, automotive-component plants, aerospace repair stations and air-conditioning manufacturers (who braze aluminium heat exchangers by the million) run vacuum furnaces. The furnace is a cold-wall vessel with a graphite or molybdenum hot zone inside; the vacuum system is what makes the atmosphere, and the atmosphere is the process.

1. What the vacuum has to do

Three things, at three stages:

  1. Pump down the cold chamber from atmosphere to the pressure at which heating may start — typically 10⁻¹ to 10⁻² mbar — in a time that does not dominate the cycle. For a 1 m³ hot zone (chamber volume 3–4 m³ with the insulation and fixtures), 10–20 minutes.
  2. Hold the process pressure against outgassing as the charge heats. Everything in the furnace gives off gas when hot: water and oil from the parts, adsorbed gases from the graphite insulation (a great deal, especially after the door has been open in Bangkok humidity), binder from sintering parts, zinc and magnesium vapour from brazing alloys. The pressure during heating is set by the balance of outgassing against the set's speed at that pressure; the specification for bright hardening of tool steel is usually < 10⁻² mbar, for aluminium brazing 10⁻⁴ to 10⁻⁵ mbar (to keep the oxide from reforming), for sintering 10⁻¹ to 10⁻² mbar with a partial pressure of nitrogen or argon.
  3. Partial-pressure operation: for high-speed steels and alloys containing chromium or manganese, holding at 10⁻⁴ mbar at 1,100 °C evaporates the alloying elements from the surface. The furnace backfills with 0.5–5 mbar of nitrogen or argon, and the pump set runs with a controlled gas bleed — a continuous throughput duty.

Then a gas quench: the chamber is backfilled to 2–20 bar of nitrogen, helium or argon and a fan circulates it over the hot charge. The pump plays no part in the quench — but it does pump the chamber down again for the next load, and on furnaces with quench gas recovery it draws the quench gas back into a storage vessel through a compressor instead of venting it.

Why does the pump-down formula fail for a furnace?

Because a furnace is not an empty vessel. The chamber volume is 3 m³, but the graphite felt insulation has an internal surface area of thousands of square metres, all of it holding adsorbed water after the door was open for loading. The pump-down proceeds normally to about 1 mbar, where the air is gone, and then slows to a crawl, limited not by the pump's speed but by the rate at which water desorbs from the insulation. A new, dry furnace reaches 10⁻² mbar in 15 minutes; the same furnace after a weekend open in the rainy season takes an hour, and no pump of any size fixes that — only heating the insulation (a low-temperature bake) or keeping the furnace closed and under vacuum between loads. Sizing the set for the empty-chamber pump-down and then adding margin for outgassing (the hold duty) is the right method; sizing it to achieve a short pump-down on a wet furnace is a waste of a large pump.

2. The pump set

A furnace vacuum system is a two- or three-stage set:

  • Backing / roughing pump: an oil-sealed two-stage rotary vane (DV Series, 5 × 10⁻³ mbar) or a dry screw (DSI Series, 0.05 mbar). It does the pump-down from atmosphere to the booster's cut-in and backs the booster afterward.
  • Roots booster (MB Series): cuts in at 30–80 mbar and gives the set its speed in the 10–10⁻³ mbar band — see When a Roots booster pays. Most hardening, tempering and sintering furnaces stop here, at an ultimate of 10⁻³–10⁻⁴ mbar with a DV backing pump.
  • Diffusion pump (oil vapour jet, 2,000–20,000 L/s): for the 10⁻⁴–10⁻⁶ mbar needed by aluminium brazing, titanium and superalloy work. Backed by the booster/DV set, with a water-cooled baffle to limit oil back-streaming. Some new furnaces use a large turbomolecular pump instead.

For the hold duty the set must have, at the process pressure, a speed of S = Q/p against the outgassing Q. A charge of 500 kg of machined tool steel plus the furnace's own insulation might outgas 5 mbar·L/s at 500 °C (mostly water, falling as it heats); holding 10⁻² mbar needs 500 L/s = 1,800 m³/h at that pressure — an MB600-class booster's territory, and a DV alone would sit at 10⁻¹ mbar.

3. Sizing a 1 m³ hot-zone hardening furnace

Chamber 3.5 m³, process 10⁻² mbar, pump-down target 15 minutes to 10⁻¹ mbar (cold, dry), hold 10⁻² against 5 mbar·L/s.

  • Roughing 1,013 → 50 mbar in 4 minutes: (3.5/0.067) × 3 ≈ 160 m³/h → a DV175 (160 m³/h) exactly; a DV275 (255 m³/h) for margin and a faster cycle.
  • Booster cutting in at 50 mbar: an MB600 (2,000 m³/h) on the DV275 is a 7.8 : 1 staging ratio; effective speed ~1,500 m³/h through the 10–0.01 mbar band; 50 → 0.1 mbar in about 1.5 minutes; hold at 10⁻² mbar against 5 mbar·L/s with ~1,200 m³/h available — comfortable.
  • Ultimate of the set ~10⁻³ mbar — adequate for hardening, tempering, annealing and most brazing of steel; not for aluminium brazing, which adds a diffusion pump.
  • Partial pressure: a mass-flow-controlled nitrogen bleed of 5–20 L/min at 1–2 mbar is a throughput of 100–400 mbar·L/s; the booster handles it; the backing pump must have the speed at its foreline pressure (the DV275 does).

The set: MB600 + DV275, pressure-switch cut-in, bypass around the booster, an inlet dust filter (graphite and oxide dust), and the backing pump's exhaust through a mist separator to outside.

4. What comes out of the charge

Process Vapour / contaminant Threat Protection
Hardening machined parts Cutting oil, water Oil in backing pump oil; water emulsion Pre-clean parts; gas ballast; oil change by hours
Sintering MIM / PM parts Binder (wax, polymer) burn-out Condenses in booster and lines as tar Heated inlet line, binder trap (cold trap) before booster, dry screw backing
Aluminium brazing Magnesium vapour (getter), flux residue Mg condenses as powder on cold surfaces, including pump inlets Mg trap / shield in furnace outlet; filter; frequent cleaning
Carburising (LPC) Acetylene / propane, soot Soot in booster and backing pump Soot filter; dry screw backing; purge
Oil quench furnaces Quench oil vapour Oil in pumps Baffle and cold trap; dedicated set

Dry screw backing pumps have become the choice on sintering and low-pressure carburising furnaces because binder and soot do not mix with pump oil; two-stage vane pumps remain on hardening and brazing furnaces where the gas is cleaner and the ultimate matters.

5. Installation and running

  • Short, large-bore pipe between chamber and set: DN100–160 for this size; every metre of DN50 throws away booster speed in molecular flow.
  • Isolation valve at the chamber so the set stays under vacuum between loads (the insulation stays dry).
  • Leak check of the chamber at commissioning and quarterly: pressure rise < 5 × 10⁻³ mbar/min for a hardening furnace, < 10⁻³ for brazing. Door seals, thermocouple feedthroughs and the power feedthroughs are the usual leaks.
  • Water cooling for the booster (gas-cooled types) and the diffusion pump; the plant room needs chilled or tower water.
  • Backing pump oil: furnace duty is hard on it; a dedicated oil management routine, and an oil heater for cold starts.
  • Interlocks: heating permitted only below set pressure; booster only below cut-in; quench only with the pump set isolated.

6. Worked furnaces

Furnace Chamber Process Dr.Vakuum set
Small tool-shop hardening, 0.3 m³ hot zone 1.2 m³ 10⁻² mbar MB150 + DV60
Hardening / tempering, 1 m³ hot zone (above) 3.5 m³ 10⁻² mbar, N₂ partial pressure MB600 + DV275
Aluminium brazing, HVAC coils, 2 m³ hot zone 7 m³ 10⁻⁵ mbar Diffusion pump + MB600 + DV275, Mg trap
MIM sintering, 0.5 m³ 2 m³ 10⁻¹–10⁻² mbar, binder burnout MB300 + binder trap + DSI150
Low-pressure carburising, 1 m³ 3.5 m³ 5–20 mbar C₂H₂, 10⁻² between MB600 + soot filter + DSI300

Recommended Dr.Vakuum machines

Roots boosters (MB Series): MB150, MB300, MB600, MB1200.

Two-stage oil-sealed vane (DV Series) — hardening and brazing backing: DV60, DV90, DV175, DV275.

Dry screw (DSI Series) — sintering and carburising backing: DSI150, DSI300.

The high-vacuum stage for brazing and coating — diffusion versus turbo versus cryo — is covered in High vacuum for coating and analytical instruments.

Furnace to set. Tell us the chamber volume, the process pressure and the cycle, and what the charge carries, and we will size the booster and backing pump, and tell you whether a diffusion stage is needed. Talk to an engineer.